Cross-Linked Shrink Film - CX


TYPICAL PROPERTIES

Gauge 45 60 75 100
Unit Test
Method
Yield Sq. in. per pound 66,000 50,000 40,000 30,000
Tensile properties: MD TD MD TD MD TD MD TD
Tensile strength N/mm² D-883 125 115 120 100 125 105 110 100
Elongation % D-884 105 100 105 100 110 107 120 115
Seal Strength N/mm² Int. meth. 71 67 65 60
Tear propagation gr D-1922 7.3 10 11.5 13
Cof. film-film, kinetic adim. D-1894 0.26 0.25 0.25 0.25
Shrink at 250°F % D-2732 MD TD
70 71
MD TD
68 69
MD TD
67 67
MD TD
66 66
Optical properties:
Haze % D-1003 1.5 1.7 2 2.4
Gloss photoc. D-2457 131 125 123 121